000 | 03181nam a22005057a 4500 | ||
---|---|---|---|
001 | sulb-eb0025968 | ||
003 | BD-SySUS | ||
005 | 20160413122558.0 | ||
007 | cr nn 008mamaa | ||
008 | 120913s2013 ii | s |||| 0|eng d | ||
020 |
_a9788132207207 _9978-81-322-0720-7 |
||
024 | 7 |
_a10.1007/978-81-322-0720-7 _2doi |
|
050 | 4 | _aTA401-492 | |
072 | 7 |
_aTGM _2bicssc |
|
072 | 7 |
_aTNC _2bicssc |
|
072 | 7 |
_aTEC021000 _2bisacsh |
|
082 | 0 | 4 |
_a620.11 _223 |
100 | 1 |
_aSaha, Jayanta Kumar. _eauthor. |
|
245 | 1 | 0 |
_aCorrosion of Constructional Steels in Marine and Industrial Environment _h[electronic resource] : _bFrontier Work in Atmospheric Corrosion / _cby Jayanta Kumar Saha. |
264 | 1 |
_aIndia : _bSpringer India : _bImprint: Springer, _c2013. |
|
300 |
_aXX, 176 p. _bonline resource. |
||
336 |
_atext _btxt _2rdacontent |
||
337 |
_acomputer _bc _2rdamedia |
||
338 |
_aonline resource _bcr _2rdacarrier |
||
347 |
_atext file _bPDF _2rda |
||
490 | 1 |
_aEngineering Materials, _x1612-1317 |
|
505 | 0 | _aTheoretical Evidences -- Practical Approach -- Experimental Evidence -- Analysis. | |
520 | _aThe book entails investigative methods for better understanding of the degradation process and uses of high performance paints formulation and also compares them on mild steel (MS) and weathering steel (WS) through various AC/DC electrochemical test methods and surface characterization through electron microscopy, XRD and Raman spectroscopy. This book also deals with the corrosion studies undertaken considering three phases (solid, liquid and gas) with latest techniques and the emphasis has also been given on degradation of materials due to atmospheric corrosion as this is of immense interest to present engineers and researchers. MS has got versatile application as structural steel for construction of buildings, bridges, flyovers, pipelines etc. But this is very much prone to corrosion in industrial and marine environments in presence of harmful pollutants and other industrial effluents in addition to normal humid atmosphere. These corrosion problems are much severe in a tropical country like India with vast coastline. MS corrodes relatively faster and thus leads to colossal loss in every year and to reduce this loss some kind of protection in the form of paints and coatings is always used. Painting is an effective means but quite costly amounting 10-15% of the initial construction cost of superstructures besides cost of repainting at regular interval. | ||
650 | 0 | _aMaterials science. | |
650 | 0 | _aElectrochemistry. | |
650 | 0 | _aChemical engineering. | |
650 | 0 | _aStructural materials. | |
650 | 1 | 4 | _aMaterials Science. |
650 | 2 | 4 | _aStructural Materials. |
650 | 2 | 4 | _aIndustrial Chemistry/Chemical Engineering. |
650 | 2 | 4 | _aElectrochemistry. |
710 | 2 | _aSpringerLink (Online service) | |
773 | 0 | _tSpringer eBooks | |
776 | 0 | 8 |
_iPrinted edition: _z9788132207191 |
830 | 0 |
_aEngineering Materials, _x1612-1317 |
|
856 | 4 | 0 | _uhttp://dx.doi.org/10.1007/978-81-322-0720-7 |
912 | _aZDB-2-CMS | ||
942 |
_2Dewey Decimal Classification _ceBooks |
||
999 |
_c48060 _d48060 |